Æȷοì
mehrdad kokabi
mehrdad kokabi
modares.ac.irÀÇ À̸ÞÀÏ È®ÀÎµÊ - ȨÆäÀÌÁö
Á¦¸ñ
Àοë
Àοë
¿¬µµ
PVA–clay nanocomposite hydrogels for wound dressing
M Kokabi, M Sirousazar, ZM Hassan
European polymer journal 43 (3), 773-781, 2007
8322007
Ablation and thermal degradation behaviour of a composite based on resol type phenolic resin: process modeling and experimental
AR Bahramian, M Kokabi, MHN Famili, MH Beheshty
Polymer 47 (10), 3661-3673, 2006
2012006
Ablation mechanism of polymer layered silicate nanocomposite heat shield
AR Bahramian, M Kokabi
Journal of Hazardous Materials 166 (1), 445-454, 2009
1382009
Conductive bacterial cellulose/multiwall carbon nanotubes nanocomposite aerogel as a potentially flexible lightweight strain sensor
H Hosseini, M Kokabi, SM Mousavi
Carbohydrate polymers 201, 228-235, 2018
1322018
A biosynthetic nerve guide conduit based on silk/SWNT/fibronectin nanocomposite for peripheral nerve regeneration
F Mottaghitalab, M Farokhi, A Zaminy, M Kokabi, M Soleimani, ...
PloS one 8 (9), e74417, 2013
1282013
Shape memory and mechanical properties of cross-linked polyethylene/clay nanocomposites
S Rezanejad, M Kokabi
European polymer journal 43 (7), 2856-2865, 2007
1132007
The effect of composition and draw-down ratio on morphology and oxygen permeability of polypropylene nanocomposite blown films
A Mirzadeh, M Kokabi
European Polymer Journal 43 (9), 3757-3765, 2007
1072007
Poly (vinyl alcohol)/chitosan/honey/clay responsive nanocomposite hydrogel wound dressing
S Noori, M Kokabi, ZM Hassan
Journal of Applied Polymer Science 135 (21), 46311, 2018
1012018
The role of interfacial interactions on the glass-transition and viscoelastic properties of silica/polystyrene nanocomposite
M Mortezaei, MHN Famili, M Kokabi
Composites science and technology 71 (8), 1039-1045, 2011
912011
Drying of gelcast ceramic parts via the liquid desiccant method
A Barati, M Kokabi, MHN Famili
Journal of the European Ceramic Society 23 (13), 2265-2272, 2003
872003
Swelling behavior and structural characteristics of polyvinyl alcohol/montmorillonite nanocomposite hydrogels
M Sirousazar, M Kokabi, ZM Hassan
Journal of Applied Polymer Science 123 (1), 50-58, 2012
862012
Design, manufacturing and evaluation of the performance of steel like fiber reinforced elastomeric seismic isolators
GD Ashkezari, AA Aghakouchak, M Kokabi
Journal of materials processing technology 197 (1-3), 140-150, 2008
862008
Nanoclay enhanced the mechanical properties of poly (vinyl alcohol)/chitosan/montmorillonite nanocomposite hydrogel as wound dressing
S Noori, M Kokabi, ZM Hassan
Procedia Materials Science 11, 152-156, 2015
812015
High temperature ablation of kaolinite layered silicate/phenolic resin/asbestos cloth nanocomposite
AR Bahramian, M Kokabi, MHN Famili, MH Beheshty
Journal of hazardous materials 150 (1), 136-145, 2008
772008
Sound barrier properties of sustainable waste rubber/geopolymer concretes
M Gandoman, M Kokabi
Iranian polymer journal 24, 105-112, 2015
742015
Non-linear free vibrations of Kelvin–Voigt visco-elastic beams
SN Mahmoodi, SE Khadem, M Kokabi
International Journal of Mechanical Sciences 49 (6), 722-732, 2007
732007
Gelation process in low-toxic gelcasting systems
M Kokabi, AA Babaluo, A Barati
Journal of the European Ceramic Society 26 (15), 3083-3090, 2006
732006
High performance flexible actuator: PVDF nanofibers incorporated with axially aligned carbon nanotubes
S Sharafkhani, M Kokabi
Composites Part B: Engineering 222, 109060, 2021
682021
BC/rGO conductive nanocomposite aerogel as a strain sensor
H Hosseini, M Kokabi, SM Mousavi
Polymer 137, 82-96, 2018
602018
In vivo and cytotoxic assays of a poly (vinyl alcohol)/clay nanocomposite hydrogel wound dressing
M Sirousazar, M Kokabi, ZM Hassan
Journal of Biomaterials Science, Polymer Edition 22 (8), 1023-1033, 2011
602011
ÇöÀç ½Ã½ºÅÛÀÌ ÀÛµ¿µÇÁö ¾Ê½À´Ï´Ù. ³ªÁß¿¡ ´Ù½Ã ½ÃµµÇØ ÁÖ¼¼¿ä.